    面对环氧树脂地坪失光现象应该怎么处理

    发布时间:2023-05-13 浏览:704次 字号:  

    环氧地坪漆的优点是与基层的粘接强度高,硬化时收缩率极低,不易开裂;整体无缝,易清洗,不集聚灰尘、细菌;强度高,耐磨损,经久耐用;抗渗透,耐化学药品的腐蚀性能强,对油类也有较好的容忍力;室温固化成膜,容易维修保养;表面平整光滑,色彩丰富,能美化工作环境、地面无毒,符合卫生要求。环氧地坪漆失光了怎么办,不要着急,环氧地坪漆来教你如何避免和处理环氧树脂地坪的失光。

    The advantages of epoxy floor paint are high bonding strength with the base, low shrinkage rate during hardening, not easy to crack; seamless, easy to clean, not gathering dust and bacteria; high strength, wear resistance, durable; anti-penetration, chemical resistance, corrosion resistance, and good tolerance to oils; room temperature curing film forming. Easy maintenance; smooth surface, rich color, beautifying the working environment, non-toxic ground, in line with health requirements. What if the epoxy floor paint loses its gloss? Don't worry. The epoxy floor paint teaches you how to avoid and deal with the gloss of the epoxy floor. 

    1、环氧地坪漆物面处理不干净,含有酸、碱、油污、蜡质和水分等。这就要求我们施工前,被涂物表面应充分处理干净。

    1. The surface treatment of epoxy floor paint is not clean. It contains acid, alkali, oil, wax and water. This requires that before construction, the surface of the coating should be fully treated and cleaned.

    2、被涂物表面过分粗糙或多孔,未涂封闭底漆会发生环氧地坪失光现象。此种原因引起的环氧树脂地坪失光就需要我们物面应用底漆封闭,腻子填平,打磨。

    2. The surface of the coated material is too rough or porous, and the epoxy floor will lose its gloss if the primer is not sealed. The loss of gloss of epoxy floor caused by this kind of reason requires us to apply primer to seal the surface, fill the putty and polish it.

    3、施工场所湿度太大(相对湿度超过85%),挥发性漆的涂膜容易吸收水分而发白发光。预防:施工场所的湿度不宜过大。

    3. The humidity of the construction site is too high (relative humidity is over 85%). The film of volatile paint is easy to absorb moisture and emit white light. Prevention: The humidity of construction site should not be too high.

    4、涂膜软,耐划伤性能不好。预防:按被涂物的使用条件,选用耐候性、抗划伤性能良好的涂料。

    4. The coating is soft, and the scratch resistance is not good. Prevention: According to the application conditions of the coatings, the coatings with good weatherability and scratch resistance are selected.

    5、漆中颜料的水分含量过高或施工中混入水分。

    5. The moisture content of paint is too high or mixed with water in construction.

    6、预防:应控制颜料的含水量,施工中避免混入水分。

    6. Prevention: Water content of pigments should be controlled to avoid mixing in water during construction.

    7、施工中稀释剂用量过多或加入了煤油一类的高沸点稀释剂。预防:稀释剂用量不宜过多,应避免煤油一类的高沸点溶剂的加入。

    7. Excessive amount of diluent or high boiling point diluent such as kerosene are added in construction. Prevention: The dosage of diluent should not be too much, and the addition of high boiling point solvent such as kerosene should be avoided.

    8、涂膜未完全干透之前遇雨水或露水。预防:涂膜在干燥过程中要防止雨水或露水浸润。

    8. Rainwater or dew will be encountered before the film is completely dried. Prevention: The film should prevent rain or dew from soaking in the drying process.

    根据以上分析可以看出,环氧地坪漆环氧地坪的施工技术和习惯是造成失光的重要原因之一,养成规范的施工技术和施工环境要求,按标准施工流程操作就可以避免防治环氧树脂地坪漆出现失光机率。

    According to the above analysis, it can be seen that the construction technology and habits of epoxy floor paint is one of the important reasons for the loss of light. Forming the standard construction technology and construction environment requirements, according to the standard construction process operation can avoid preventing and curing the loss of light of epoxy floor paint.